Titanium Anodes For Chemical Processes

Coating Chosen By Process,
Not By Price

Home  /  Applications  /  Chemical Industry

Two Reactions,
Two Coating Families

A chemical cell asks one question of its anode: does it evolve chlorine or oxygen? The answer decides the coating chemistry, and getting it wrong shortens service life from years to months.

Ehisen supplies MMO coated titanium anodes for both families — ruthenium-based systems for chlorine evolution (chlor-alkali, chlorate, hypochlorite, chlorine dioxide) and iridium-based systems for oxygen evolution (perchlorate, persulfate, chromium salts, organic oxidation). Where the electrolyte is strongly acidic and oxidising, an intermediate layer is added between substrate and active coating to hold the layer in place.

Tell us the electrolyte, temperature and current density. We match substrate grade, coating system, active area and connection detail, then confirm the basis in the quotation.

Product Forms

Four ways an anode reaches your cell

MMO Coated Plate

Ruthenium or iridium mixed-metal-oxide coating on titanium plate. The standard form for chlor-alkali cells, chlorate reactors and plate-type oxidisers.

Titanium Mesh Anode

Expanded or woven mesh with double-sided coating. Used where flow-through and high surface area matter, including electrochlorination and cathodic protection.

Felt & Porous Plate

Three-dimensional titanium felt or sintered porous sheet, coated on both faces. Specified by external dimensions and porosity for high-area electrodes.

Custom Platinum Parts

Platinum-coated titanium components machined to drawing, including shapes that cannot be produced as flat plate or standard mesh.

Why It Matters

0.75 V is the difference between a consumable and a component

Replacing graphite with a coated titanium anode in the same diaphragm cell drops cell voltage from 4.00 V to 3.25 V. The saving splits into two measurable parts: anodic overpotential and conductor drop.

Because the anode no longer dissolves, the gap between electrodes can be held constant — which is what allows current density to rise without the cell drifting out of its design window.

Note on data: figures shown are industry-literature values used to explain the mechanism. Product performance is stated per batch in the COA and test report.
Graphite anodeCoated titanium anode
Graphite
4.00 V
100%
Coated Ti
3.25 V
81%
Anodic overpotential 0.33 V → 0.02 V. Metal conductor drop 0.36 V → 0.17 V. Cathode and electrolyte terms are unchanged.
Application Map

Nine chemical processes, nine operating windows

Similar-looking anodes behave differently according to the reaction they are asked to drive. Use the table to locate your process, then open the matching chapter below.

ProcessMain reactionCoating familyTypical condition
Chlor-alkali (diaphragm / membrane / mercury)Chlorine evolutionRuTi, RuIr30–40 A/dm² · ~3.1 V
ChlorateChlorine evolutionRuTi, RuIr, RuIrSn1500–4000 A/m² · 60–90 °C
Hypochlorite (on-site generator)Chlorine evolutionFive-element oxide13–20 A/dm² · <40 °C
Chlorine dioxideChlorine evolutionMMO (generator system)On-site generation
PerchlorateOxygen evolutionIridium-based15–50 A/dm² · 35–50 °C
Persulfate / hydrogen peroxideOxygen evolutionPlatinum, Ti/IrO&sub2;70–120 A/dm²
Chromium saltsOxygen evolutionTi/IrO&sub2;+Ta&sub2;O&sub5;; PbO&sub2; with interlayerHigh current density
Organic electrosynthesisReaction-dependentRuO&sub2;, Ir, Pt, PbO&sub2;Process-specific
Chemical wastewater oxidationOxygen evolutionMMO (oxidation duty)Chloride-dependent
Selection Basis

Four criteria we apply before quoting

01

Chlorine selects ruthenium, oxygen selects iridium

In oxygen-evolution duty a ruthenium coating oxidises into soluble species and leaves the surface. The reverse error costs efficiency rather than life, but both should be avoided by matching the reaction first.

02

The gap between chlorine and oxygen potential matters more than either value

A low chlorine-evolution potential alone does not indicate a good coating. What controls current efficiency is how far the oxygen-evolution potential sits above it, because that gap suppresses the competing reaction.

03

Strong acid plus strong oxidation requires an interlayer

Where an active layer would otherwise lift, we introduce an oxide interlayer that shares the rutile structure with both substrate and active phase, so the stack is chemically continuous rather than merely painted on.

04

Temperature and gap limits are set by the anode, not the equipment

Graphite in a chlorate cell is held near 40 °C and cannot maintain a close gap; a coated titanium anode operates at 60–90 °C with a stable gap in the 2–5 mm range. Any proposal to raise temperature or current density is really a question about the anode.

Process Chapters

Working notes by application

Open the chapter that matches your cell. Each note states the reaction, what the anode has to survive, the coating family we would propose and the failure pattern to watch for.

Reaction. Chlorine evolution at the anode; hydrogen and hydroxide at the cathode. Three routes are in service: diaphragm (caustic 100–140 g/L), membrane (perfluorinated film passing Na&sup+; only) and mercury (sodium amalgam intermediate).

What the anode must survive. Chlorine and hypochlorous acid attack, continuous DC, large plate area with a stable gap, and years of service between recoating cycles.

Coating we would propose. Ruthenium-based MMO, typically RuTi for diaphragm duty and RuIr where current density is higher. Mercury cells run hotter and at much higher current density, so the formulation is adjusted accordingly.

Failure pattern. Cell voltage creeping upward with efficiency unchanged usually means the gap has moved or the coating is being consumed — both are visible in a voltage log long before a physical inspection.

Reaction. NaCl + 3H&sub2;O → NaClO&sub3; + 3H&sub2; in an undivided cell on saturated brine. Cathodic hydrogen raises pH; dissolved chlorine converts through hypochlorous acid to chlorate.

What the anode must survive. 60–90 °C, 1500–4000 A/m², and a gap that must stay in the 2–5 mm range. Graphite is limited to roughly 40 °C and cannot hold a close gap because it erodes.

Coating we would propose. Ruthenium-based MMO, with RuIr or RuIrSn where the operating window demands higher loading.

Failure pattern. Localised coating burn-off at the current-density peak, and accelerated consumption when temperature is pushed beyond the coating’s tolerance rather than the equipment’s.

Reaction. Undivided electrolysis of dilute brine. On-site generators run 3–5% salt and produce 6–10 g/L available chlorine, avoiding the transport and storage of concentrated hypochlorite.

What the anode must survive. Low chloride concentration, temperature below 40 °C, neutral pH and a narrow gap. Magnesium in the feed water precipitates as hydroxide on the anode surface and drives crevice corrosion of the titanium substrate beneath it.

Coating we would propose. Five-element mixed oxide systems developed for low-salinity duty. For hard feed water we discuss a platinum interlayer, which is the practical answer to hydroxide blanketing.

Failure pattern. White deposit on the active face followed by pitting of the substrate. If the deposit is present, the coating is usually still serviceable while the substrate is not.

Sanitation note. For drinking-water disinfection, electrode materials must not introduce chromium or lead. Graphite and lead-dioxide coatings are therefore excluded from that duty.

Reaction. Chlorate oxidises to perchlorate at the anode (1.19 V standard); sulfate oxidises to persulfate, which is then hydrolysed to hydrogen peroxide. In both cases oxygen evolution competes directly with the wanted reaction.

What the anode must survive. Sulfuric acid media, high current density, and the need for a high oxygen-evolution overpotential so the parasitic reaction is suppressed rather than merely outrun.

Coating we would propose. Iridium-based MMO where a durable oxide is required; platinum or platinum-coated titanium where the highest oxygen overpotential is needed and the platinum consumption can be tolerated.

Failure pattern. Platinum layers blister and detach after long runs, with efficiency fading gradually. This is characteristic of the platinum family and should be planned for in the replacement cycle.

Reaction. Trivalent chromium is oxidised to dichromate, either directly or through a mediator; organic electrosynthesis covers amino acids, epoxides and ring chlorination.

What the anode must survive. Sulfuric acid plus strong oxidation, the combination that lifts a lead-dioxide layer off a bare substrate. In organic duty the anode may also dissolve at the potentials required.

Coating we would propose. For dichromate synthesis we propose IrO&sub2; + Ta&sub2;O&sub5;, which holds up in acid oxidising media. Where a lead-dioxide active phase is required by the process, it is deposited over an oxide interlayer that shares the rutile structure with the substrate, so the stack stays bonded.

Failure pattern. Sheet-like detachment of the active layer with the substrate exposed and bright. Once the interlayer is breached the remaining coating goes quickly.

Troubleshooting

Five ways an anode fails before its time

Most early failures are a mismatch between coating and duty rather than a manufacturing defect. Match the symptom before ordering a replacement.

01 / Blistering

Platinum layer lifts

Symptom
Local blisters, then sheet detachment; efficiency falls month by month
Cause
Long service under strong oxidising duty
Action
Control current density and stops; plan recoating
02 / Delamination

Active layer peels

Symptom
Coating lifts as a sheet, bright substrate underneath
Cause
Acid plus oxidation without an interlayer
Action
Specify an oxide interlayer in the stack
03 / Crevice

Substrate corrodes under deposit

Symptom
White hydroxide film, then pitting through the titanium
Cause
Hard feed water in hypochlorite duty
Action
Platinum interlayer; control feed hardness
04 / Blockage

Channel plugged with debris

Symptom
Rising cell voltage, local hot spots
Cause
Eroded graphite particles collecting in the gap
Action
Move to an insoluble coated anode
05 / Drift

Voltage drifts with efficiency intact

Symptom
Slow voltage rise over months, production unchanged
Cause
Gap change from erosion, or overpotential rise from coating loss
Action
Dimensionally stable anode; log overpotential
Specification

What we confirm before production

Anode properties are set per project. The table lists the fields we settle with you; values are stated in the quotation and repeated in the COA.

ParameterBasisStated in
Substrate gradeTitanium grade selected against electrolyte and forming requirementDrawing / quotation
DimensionsLength × width × thickness to your cell drawing; active area markedApproved drawing
Mesh / porosityMesh count or porosity for mesh, felt and porous plate formsApproved drawing
Coating systemRu-based, Ir-based, five-element mixed oxide, or platinumQuotation
Noble-metal loadingg/m² set by duty; loading drives coat count and sintering profileCOA
Coating thicknessMeasured per batchCOA
Chlorine-evolution potentialMeasured against reference electrode; test medium and temperature statedTest report
Accelerated lifeHours to failure under stated current density and acid conditionsTest report
Coating uniformityDistribution across active areaTest report
PackingFace protection, moisture barrier, crate fixing to drawingPacking list
Lead timeQuoted per order against drawing approval dateQuotation
DocumentsCOA, packing list, test report; third-party testing on requestPer order
Two fields are commonly misunderstood. Purity does not apply to a fabricated metal electrode — what matters is substrate composition and coating loading. CAS numbers likewise apply to precursor chemicals, not to the finished anode, so we issue a COA against loading and potential instead.
FAQ

Questions we are asked before a first order

Start from the reaction, not the coating name. If the anode mainly evolves chlorine — chlor-alkali, chlorate, hypochlorite, chlorine dioxide — the ruthenium family applies. If it mainly evolves oxygen — perchlorate, persulfate, chromium salts, organic oxidation — the iridium family applies. Mixed duty needs the duty cycle examined, and we would review that with you.

Mesh, felt and porous plate are normally coated on both faces. Single-sided coating changes the field distribution and the way the substrate is protected, so we assess it before confirming feasibility rather than committing in advance.

Life is a function of coating loading, current density, temperature and electrolyte purity — not a single catalogue number. Industry experience for hypochlorite duty from seawater is measured in years, and chlor-alkali anodes are planned in years between recoating. A realistic figure needs your operating window.

Application and target reaction, electrolyte composition with pH and temperature, current density and operating voltage, drawing or dimensions, quantity and document requirements. A photograph of the used anode is often the fastest way to establish the replacement geometry.

Yes. We handle substrate machining, coating, assembly, marking and export packing against your drawing. Dimensions, current path, active area and installation detail are reviewed at the first drawing check.

A COA is issued per batch against noble-metal loading, coating thickness, potential and appearance. For the safety data sheet we state the position in writing against the actual materials used rather than assuming a classification.

Send The Data That Matters

Tell us the cell.
We will tell you the coating.

You do not need a complete drawing or every parameter. Send what you know and we will confirm the rest before quoting.

Request a technical review

Typical reply within one working day.

Used for this enquiry only. Coating selection is confirmed after technical review and, where needed, sample evaluation.